EN 14700: TNi2
DIN 85551: MSG 23-GF-200/350-CKNTZ
1 Former classification replaced by EN 14700
• Cobalt hardened super-alloy metal-cored wire of the NiCrMoW type
• Particularly resistant to corrosion under oxidising and reducing atmospheres
• Weld metal is designed to withstand impact, compression, abrasion, oxidation, corrosion and heat up to 1100°C
• Excellent thermal shock resistance
• Can be machined without previous heat treatment
STELLOY CCo-G is suitable for surfacing parts undergoing oxidation, corrosion and mechanical stresses at high temperature
Examples
Tube extrusion mandrels, hot shearing blades, extrusion tooling, forging dies.
TYPICAL ALL-WELD METAL ANALYSIS
CMnSiCrMoFeWCoNi
0.05
|
1.00
|
0.60
|
15.50
|
16.00
|
3.00
|
4.40
|
2.30
|
Bal.
|
Structure: solid solution of the austenitic type
TYPICAL ALL-WELD METAL MECHANICAL PROPERTIES
Hardness -3 layers deposit on mild steel:
As welded: 220 HB
Work hardened: 350 HB
l1 according to EN ISO 14175 (pure Argon)
Current typeGas flow rateRecovery
DC(+) or pulsed
|
10 - 20 l/min
|
98%
|
Diameter [mm] Amperage [A] Voltage [V] Stick-out [mm]
|
Range
|
Optimum
|
Range
|
Optimum
|
Range
|
Optimum
|
1.6
|
140 - 300
|
250
|
22 - 28
|
28
|
15 - 25
|
20
|
2.4
|
280 - 350
|
300
|
26 - 30
|
28
|
15 - 25
|
20
|
Recovery: 98 %
EN ISO 6947: PA, PB, PC
ASME IX: 1G, 1F, 2F
1.6, 2.4 mm
Other diameters: please consult us
Diameter ≤ 2.4 mm ≥ 2.4 mm
Standard packaging
|
Spool EN ISO 544: BS 300
|
Coil EN ISO 544: C450
|
Weight
|
15 kg
|
25 kg
|